A sealed aluminium enclosure is decided by three things long before it reaches the water tank: the groove geometry, the gasket section and the pitch of the fasteners that clamp them together. Get any of the three wrong and no amount of tightening will help. We machine the groove into the extrusion or the lid seat, specify the gasket to a national-standard hardness and compression set, and then test the finished unit under water rather than testing a bare box.
What each IP rating actually demands
Ingress protection is defined by GB/T 4208, which is technically equivalent to IEC 60529. The numbers that matter for an aluminium housing:
| Rating | Test | What it means in practice |
|---|---|---|
| IP65 | Water jets from a nozzle, 12.5 l/min at 30 kPa | Outdoor rain and wash-down from any direction |
| IP66 | Powerful jets, 100 l/min at 100 kPa | Hose-down, heavy spray, deck wash |
| IP67 | Temporary immersion, 1 m for 30 min | Short flooding, a dropped unit in a sump |
| IP68 | Immersion deeper than 1 m, duration and depth agreed between buyer and supplier | Continuous or repeated immersion — the depth and time must be written on the drawing |
IP65 to IP67 is our standard range. IP68 is quoted against an agreed depth and duration rather than as a blanket claim, because the two numbers are part of the specification: the same housing that holds 2 m for an hour is not automatically good for 10 m for a week.
Groove geometry
The groove is machined, so its dimensions are the one part of the seal that can be held to tolerance. These are the rules we design to, and the numbers are fixed on the drawing before a single part is cut:
| Parameter | Design rule | Why |
|---|---|---|
| Groove depth | 70–80% of gasket thickness | Sets the working compression at clamp-up |
| Groove width | Gasket width plus 0.1–0.2 mm | Allows the rubber somewhere to go when compressed |
| Compression | 20–30% of section height | Below 20% it will not seal; above 30% it takes a permanent set |
| Fill ratio | Not more than 85% of groove volume | Higher and the gasket hydraulically locks, so the lid stands off |
| Groove finish | Machined, deburred, no coating inside | Powder in the groove changes the compression by more than the tolerance |
| Corner radius | Moulded corners or a continuous die-cut loop | Cut-and-glued corners are the first leak path |
Gasket materials and hardness to national standard
Hardness is specified and accepted in Shore A to GB/T 531.1, and compression set to GB/T 7759.1 (70 °C × 24 h) — the two figures that actually predict whether a seal survives a few hundred thermal cycles. Tensile properties are checked to GB/T 528 and fluid resistance to GB/T 1690 where the application calls for it.
| Material | Shore A (GB/T 531.1) | Service temperature | Compression set (GB/T 7759.1) | Chosen for |
|---|---|---|---|---|
| EPDM | 60 ± 5 | −40 to +120 °C | ≤ 25% | Outdoor and UV exposure, water and steam, general enclosures |
| Silicone (VMQ) | 60 ± 5 | −60 to +200 °C | ≤ 25% | Wide temperature range, cold-store and high-temperature electronics |
| FKM (fluorocarbon) | 70 ± 5 | −20 to +200 °C | ≤ 20% | Oil, fuel and chemical contact, engine-bay electronics |
Hardness is not a detail. A 70 Shore A gasket in a groove designed for 60 needs roughly 40% more clamp force to reach the same compression, which on a 1.5 mm wall lid means the lid bows between the screws and the seal opens in the middle. If a customer's approved gasket is harder than the drawing assumes, the groove is what has to change.
Fastener pitch and shell stiffness
Sealing pressure comes from the screws, so the distance between them is a sealing parameter, not a mechanical afterthought. We check the deflection of the lid between fasteners against the compression the gasket needs, which usually drives either a thicker lid section, a return flange, or an extra screw — decided at DFM stage rather than discovered in the water tank. Stamped or extruded stiffening ribs are often cheaper than adding fasteners.
How we test
The unit that goes into the tank is the production configuration: the real gasket, the production fasteners and the actual cable set installed. A bare box that passes immersion only proves the groove geometry is right and says nothing about the assembly.
- For an IP68 enquiry the depth and duration come from your drawing, as set out in GB/T 4208 (technically equivalent to IEC 60529). We agree the protocol with you before tooling rather than quoting a fixed depth and time.
- The test is hydrostatic immersion: the unit is submerged, held, then opened and inspected for ingress.
- We do not substitute an air-pressure decay or leak-down check for immersion. A pressure test tells you a housing is airtight; it does not tell you a sealed enclosure survives being under water.
- Inspection records ship with the batch, and the same test is repeated on production samples through the run.
Failure modes we design out
- Groove too shallow for the gasket section — the lid stands off and the joint is metal-to-metal with no compression left.
- Powder coat inside the groove — 80 µm of coating on both faces consumes the entire compression allowance, so the groove is masked.
- Hard gasket, thin lid — the lid bows between screws and the seal opens exactly where nobody looks.
- Cable glands and connectors — the weakest point of a sealed enclosure is rarely the lid; it is the entry.
- Cut-and-glued corners — a joint line in a gasket loop is a leak path; we use moulded corners or a die-cut continuous loop.
Questions buyers ask
Can you guarantee IP68 on a standard enclosure?
No, and any supplier who says yes without asking for a depth and a duration is guessing. IP68 is defined by an agreed depth and time, so we quote it against those two numbers and test the finished unit to them.
Do you use air-pressure testing instead of immersion?
No. Our acceptance test is hydrostatic immersion of the finished unit. A pressure-decay check is a production convenience for some products, but it is not evidence that a sealed enclosure survives immersion.
What are the best gasket materials for IP67 rated enclosures?
For IP67, EPDM at 60 Shore A covers most outdoor and general electronics housings, silicone VMQ at the same hardness where the unit sees −40 °C to +150 °C or repeated steam, and FKM at 70 Shore A where oil, fuel or solvent is present. IP67 is a 1 m / 30 minute immersion test, so the gasket only has to hold a modest pressure differential — the usual failure is not the material but a groove that is too shallow or coated inside.
Which gasket material should I specify?
EPDM 60 Shore A covers most outdoor and general electronics enclosures. Move to silicone for a wide temperature range and to FKM where oil or fuel is present. Hardness is specified to GB/T 531.1 and compression set to GB/T 7759.1 so the part can be inspected against a number rather than a feel.
Can the groove be machined after anodising?
It should be machined before finishing and masked during it. Cutting a groove through an anodised layer exposes bare metal in the seal area, which is a corrosion site, and coating left in the groove changes the compression.
Send the enclosure drawing with the IP target, the depth and duration, and where the cables enter — we will return a groove and gasket specification with the quote.