Short answer: an IP rating answers two questions — dust and water — and nothing else. An outdoor enclosure also has to survive UV, salt fog, thermal cycling and condensation, and those four are decided by alloy, surface treatment, thermal design and venting rather than by the gasket.
Choosing the rating from the exposure
| Installation | Rating to specify |
|---|---|
| Sheltered, indoor, occasional splash | IP54 |
| Open air, rain and hose wash-down | IP65 |
| Driving rain, pressure wash, vehicle-mounted | IP66 |
| Occasional flooding, snow pack, low-level submersion | IP67 — 1 m for 30 min |
| Permanent submersion | IP68 at an agreed depth, with a pressure test |
Specifying one grade above the exposure is normal engineering margin. Specifying IP68 "to be safe" is not: it forces a different sealing architecture and a test regime that has to be repeated on every design change.
The four things IP does not cover
1. UV
Aluminium does not degrade in sunlight, but the finish can. Anodising is inherently UV-stable; powder coatings need a polyester or PVDF chemistry rather than a generic epoxy, which chalks and fades outdoors. Gaskets matter too — EPDM and silicone both resist UV and ozone, while cheap nitrile does not.
2. Salt fog
Coastal and marine sites attack the enclosure at three points: the coating itself, every fastener, and every cut edge where bare metal is exposed. The workable combination is a sealed anodic or thick powder finish, stainless fasteners, and isolating washers wherever stainless meets aluminium to break the galvanic couple. A salt-spray test on the finished assembly is the only credible evidence.
3. Thermal cycling
A sealed housing in direct sun can run far above ambient, then drop at night. That cycle works on the gasket, the sealant and any bonded window. Two consequences: pick a gasket with low compression set (silicone rather than a cheap blend), and check that the lid and body expand at similar rates — mixed materials move differently and open a gap at the extremes.
4. Condensation
This is the failure that IP ratings never catch. A sealed box breathes in humid air on a warm day, then the temperature drops, and water condenses on the inside of the lid — directly above the electronics. The fixes are a pressure-equalisation vent with an ePTFE membrane so vapour can escape without liquid entering, a desiccant pack sized to the internal volume, or conformal coating on the board itself.
Alloy and finish for outdoor service
- 6063 extrusion for constant-section outdoor housings: it anodises cleanly and forms a stable film.
- 6061 where the housing is machined from solid or needs higher strength at joints.
- Anodising where the surface has to stay dimensionally stable, dissipate heat or keep a bare contact face.
- Powder coating where colour, gloss or a thicker barrier against salt is the priority — over a conversion coat, not directly on bare metal.
- Stainless A2/A4 fasteners with isolating washers on every aluminium joint that sees weather.
Thermal management in a closed box
Sealing removes convection. An outdoor housing that was fine with vents will run hotter once it is IP67, and the derating shows up as random resets rather than an obvious failure. Three levers: use the aluminium body as the heat sink (fins outside, flat machined pads inside), couple the hottest component to the wall with a gap pad rather than air, and lower the internal heat load before adding surface area — a 10 °C reduction in load is often cheaper than 20% more fin.
Installation details that decide field life
- Mount with the lid horizontal or facing down where possible — water runs off instead of sitting on the gasket.
- Leave a drip loop in every cable entry so water cannot track along the cable into the gland.
- Keep drain paths clear at the bottom of the housing; a pocket that holds water is a corrosion cell.
- Design for service: a housing that cannot be reopened without destroying the gasket will not be maintained.
FAQ
Is IP67 enough for coastal installation?
It handles the water, not the salt. Add a finish validated by salt-spray testing, stainless fasteners with isolation, and a vent to control condensation.
Can a sealed enclosure have a breather?
Yes — a rated ePTFE vent equalises pressure while blocking liquid water, and it usually improves long-term sealing performance rather than compromising it.
Does anodising survive UV?
The anodic film itself is stable. What fades is the dye, so specify a colour-fast dye and a sealed film if appearance matters over a decade outdoors.
Send the exposure, not just the rating
Tell us where the enclosure is installed — coastal, inland, vehicle-mounted, submerged — and we will propose the rating, alloy, finish and venting that fit it, with a sample for testing before tooling.